This hybrid nanomaterial consists of multi-walled carbon nanotubes (MWCNTs) loaded with 32 wt% copper nanoparticles. It brings together the electrical conductivity and mechanical resilience of CNTs and the electrical, thermal and catalytic strengths of copper in a single black powder.
The copper phase is made of near-spherical particles with a 99.99% purity, an average size of 30 nm and a specific surface area of 40.0 m²/g, spread evenly through the nanotube network. The MWCNT component has a purity above 97 wt%, an outside diameter above 50 nm, lengths of 15-25 µm and electrical conductivity above 98 S/cm.
Distributing copper across the CNT framework yields a composite with improved hardness, tensile strength, specific strength and elastic modulus. This combination makes the material a versatile choice for research in energy storage, electronic devices, biomedical systems, catalysis and structural reinforcement.
- Electrode material for lithium-ion batteries and supercapacitors, improving conductivity, cycle stability and charge transfer, and for hydrogen storage research.
- Component in transistors, flat panel displays and solar cells to enhance charge transport and device reliability.
- Building block for biosensors, drug delivery systems and imaging nanoprobes.
- Reinforcing filler for polymer and ceramic composites aimed at aerospace, automotive and construction uses.
- Catalyst support for electrochemical and photocatalytic reactions, and use in pollutant remediation and environmental sensing.
| Brand | Nanografi |
|---|---|
| CAS number | — |
| Molecular formula | — |
| Purity | 99.99% |
| Category | — |
| Pack sizes | — |
| Physical form | — |
| Storage | — |
- Product code: NG01SC0604
- Cu content: 32 wt%
- Cu average particle size: 30 nm
- Cu specific surface area: 40.0 m²/g
- Cu true density: 9 g/cm³
- Cu shape: near spherical
- MWCNT purity: > 97 wt%
- MWCNT average outside diameter: > 50 nm
- MWCNT average inside diameter: 5 nm
- MWCNT length: 15-25 µm
- MWCNT tap density: 0.15 g/cm³
- MWCNT true density: ~2.4 g/cm³
- MWCNT specific surface area: > 65 m²/g
- MWCNT ash: < 1.5 wt%
- MWCNT electrical conductivity: > 98 S/cm
—
—