This highly conductive expanded graphite micron powder from Nanografi is a functional carbon additive with an average particle size of 20 µm and a carbon content of ≥97%. It is made by expanding natural flake graphite through chemical or electrochemical processing, giving a material that disperses evenly in host matrices and raises both thermal and electrical conductivity.
Because it keeps the core properties of crystalline graphite, the powder offers high temperature stability, corrosion resistance and self-lubricating behaviour, so it performs reliably under harsh processing and service conditions. It has a BET surface area of 30 m²/g, a tap density of 0.11 g/cm³ and a real density of 2.25 g/cm³.
In polymers, elastomers, composites and inorganic systems, the additive improves conductivity while preserving mechanical integrity, making it a cost-effective choice for durable, high-performance formulations.
- Building conductive networks in polymers and composites for charge dissipation without large increases in filler loading.
- Improving EMI/RFI shielding in housings, enclosures, coatings and electronic components.
- Raising thermal conductivity in thermally conductive plastics, heat spreaders and thermal interface materials.
- Serving as a conductive agent in electrodes for lithium-ion batteries, supercapacitors and fuel cells.
- Providing antistatic and ESD properties in elastomers and rubber compounds.
- Acting as a solid lubricant and as a precursor for graphite foil, braided packings and high-temperature seals.
| Brand | Nanografi |
|---|---|
| CAS number | 7782-42-5 |
| Molecular formula | — |
| Purity | — |
| Category | — |
| Pack sizes | — |
| Physical form | — |
| Storage | — |
- Product code: NG04EO0724
- Average Particle Size: 20 µm
- Tap Density: 0.11 g/cm³
- Real Density: 2.25 g/cm³
- BET Surface Area: 30 m²/g
- Ash Content: ≤3.0%
- Carbon Content: ≥97%
- Moisture Content (at 110 °C; 8 h): <0.5%
—
—