This lithium iron phosphate (LiFePO4, LFP) powder is a cathode active material intended for research and development work on lithium-ion batteries. It has a median particle size (D50) of 1.508 µm, a specific surface area of 12.21 m²/g and a carbon content of 1.29%, making it a practical choice for electrode formulation and electrochemical testing.
LFP owes its popularity to an olivine crystal structure, good thermal stability and the potential for long cycle life, and it uses iron and phosphorus rather than nickel or cobalt. It is one of the most studied cathode chemistries where safety, durability and cycling performance matter.
Under the manufacturer's test conditions, the powder delivered a first discharge capacity of 155.5 mAh/g with a first discharge efficiency of 97.5%. Because LiFePO4 has fairly low intrinsic electronic conductivity, it is usually combined with conductive carbon additives and a binder. Real cell performance will depend on electrode formulation, cell configuration and test protocol.
- Cathode active material for rechargeable lithium-ion battery research and electrode development.
- Research on LFP battery systems for electric vehicles and other electric mobility uses.
- Studies of rechargeable batteries for renewable, residential and grid-scale stationary energy storage.
- Cathode slurry preparation, electrode coating and optimization of active material formulations.
- Laboratory evaluation of discharge capacity, charge-discharge efficiency, cycling behavior and rate capability.
- Research on particle size distribution, conductive additives, electrode architecture and lithium-ion transport.
| Brand | Nanografi |
|---|---|
| CAS number | — |
| Molecular formula | — |
| Purity | — |
| Category | — |
| Pack sizes | — |
| Physical form | — |
| Storage | — |
- Product code: NG08BE1404
- Tap Density: 1.132 g/cm3
- Resistance: 114.9 Ω.cm
- Particle Size D10: 0.549 μm
- Particle Size D50: 1.508 μm
- Particle Size D90: 6.010 μm
- Carbon: 1.29 %
- Specific Surface Area: 12.21 m2/g
- pH: 8.92
- Moisture: 1043.0 ppm
- First Discharge Efficiency: 97.5 %
- First Capacity: 155.5 mAh/g
Keep the powder in tightly sealed containers in a clean, dry place and follow the product Safety Data Sheet (SDS). With a moisture content of 1043.0 ppm, moisture control is important for reproducible electrodes. Minimize dust and contamination using adequate ventilation, protective equipment and clean processing, and confirm any drying requirements against the manufacturer's documentation before electrode fabrication.
—